Photoplastic anisotropy in nanoindentation of wurtzite ZnO single crystals

H Hiroto Oguri (Department of Mechanical Science and Bioengineering, Osaka University 1 , Toyonaka, Osaka 560-8531,) Y Yan Li X Xufei Fang (Institute for Applied Materials, Karlsruhe Institute of Technology 1 , Karlsruhe 76131,) A Atsutomo Nakamura (Graduate School of Engineering Science, Osaka University 5 , Osaka, Toyonaka 560-8531,)

Abstract

Anisotropy plays a crucial role in understanding and optimizing the properties of materials with directional dependencies. The hexagonal wurtzite structure, which is a typical crystal structure in compound semiconductors, demonstrates pronounced anisotropy, especially in its response to external stimuli. Recently, mechanical behavior under light illumination has attracted increasing interest especially in semiconductor compounds. In this study, we investigated the anisotropy of illumination effects on the nanomechanical properties of wurtzite ZnO. Four surface orientations—(0001), (0001) 45° off, (11¯00), and (21¯1¯0)—were subjected to nanoindentation creep and nanoindentation hardness tests under controlled light illumination. The indentation depth during nanoindentation creep under light illumination was consistently smaller than that in darkness for all surface orientations, confirming that light suppresses indentation creep deformation, but to different degrees depending on the surface orientation. This suggests that the activated slip systems and the distribution of dislocations play a crucial role in modulating dislocation behavior under light illumination. The nanoindentation hardness followed the trend on the four surface orientations: (0001) > (0001) 45° off > (11¯00) > (21¯1¯0), reflecting anisotropic behavior in nanomechanical properties. Second and subsequent pop-in events were extracted, exhibiting different behaviors depending on the surface orientations, and may play a key role in determining the anisotropy in nanoindentation hardness. Our findings contribute to a comprehensive understanding of the plastic anisotropy under light control in wurtzite ZnO.

Article Details

Volume / Issue Vol. 126, Issue 11
Published March 01, 2025
ISSN 0003-6951
Publisher American Institute of Physics

Journal Info

Applied Physics Letters

American Institute of Physics

ISSN: 0003-6951 Physical Sciences

Authors (4)

H

Hiroto Oguri

Department of Mechanical Science and Bioengineering, Osaka University 1 , Toyonaka, Osaka 560-8531,

Y

Yan Li

X

Xufei Fang

Institute for Applied Materials, Karlsruhe Institute of Technology 1 , Karlsruhe 76131,

A

Atsutomo Nakamura

Graduate School of Engineering Science, Osaka University 5 , Osaka, Toyonaka 560-8531,