Galvanic Corrosion of Lithium Metal Anodes in Lithium–Sulfur Batteries

C Chen-Xi Bi (School of Materials Science and Engineering) Y Yu-Jie Zhu (School of Materials Science and Engineering) X Xi-Yao Li (Beijing Key Laboratory of Complex Solid State Batteries & Tsinghua Center for Green Chemical Engineering Electrification, Department of Chemical Engineering) J Jin Ma (Beijing Key Laboratory of Complex Solid State Batteries & Tsinghua Center for Green Chemical Engineering Electrification, Department of Chemical Engineering) X Xue-Qiang Zhang (School of Interdisciplinary Science) M Meng Zhao B Bo-Quan Li (School of Interdisciplinary Science) J Jia-Qi Huang

Article Details

Volume / Issue Vol. 147, Issue 38
Published September 24, 2025
Pages 34632-34640
ISSN 0002-7863
Publisher American Chemical Society

Journal Info

Journal of the American Chemical Society

American Chemical Society

ISSN: 0002-7863 Physical Sciences

Authors (8)

C

Chen-Xi Bi

School of Materials Science and Engineering

Y

Yu-Jie Zhu

School of Materials Science and Engineering

X

Xi-Yao Li

Beijing Key Laboratory of Complex Solid State Batteries & Tsinghua Center for Green Chemical Engineering Electrification, Department of Chemical Engineering

J

Jin Ma

Beijing Key Laboratory of Complex Solid State Batteries & Tsinghua Center for Green Chemical Engineering Electrification, Department of Chemical Engineering

X

Xue-Qiang Zhang

School of Interdisciplinary Science

M

Meng Zhao

B

Bo-Quan Li

School of Interdisciplinary Science

J

Jia-Qi Huang