C Canglong Li (School of Minerals Processing and Bioengineering Central South University Changsha China) T Tiancheng You (State Key Laboratory of Powder Metallurgy Central South University Changsha China) C Changding Wang (Institute of Future Technology Southwest Jiaotong University Chengdu China) A Antai Zhu (State Key Laboratory of Powder Metallurgy) C Changye Mang (School of Minerals Processing and Bioengineering Central South University Changsha China) H Huaming Yu Y Yang Huang (Guizhou Provincial Key Laboratory of Innovation and Manufacturing for Pharmaceuticals, School of Pharmacy) Y Yuejiao Chen G Guanghui Li L Libao Chen (State Key Laboratory of Powder Metallurgy)

Abstract

ABSTRACT The commercialization of aqueous zinc ion batteries (AZIBs) is severely hindered by the thermodynamic instability of the Zn anode interface, which leads to uncontrollable dendrite growth and parasitic side reactions. While ferroelectric polymers like poly(vinylidene fluoride) (PVDF) show promise for regulating ion flux via their built‐in electric field, the common α‐phase PVDF exhibits random dipole alignment, resulting in a negligible macroscopic polarization effect. This work demonstrates that incorporating zinc sulfide (ZnS) as a multifunctional filler is an effective strategy to actuate a crucial phase transformation from the non‐polar α‐phase to the highly polar β‐phase within the PVDF matrix. The resulting dipole‐enhanced hybrid layer (DEHL) features a structure where β‐phase nanocrystalline domains are aligned akin to “dipole superstructures,” generating a strong and homogeneous built‐in electric field. This field functions as an intelligent regulator, steering Zn 2+ ions toward uniform nucleation and dense deposition while simultaneously repelling SO 4 2− anions, thus synergistically suppressing zinc dendrites and inhibiting byproduct formation. Consequently, the DEHL‐protected Zn anode (DEHL@Zn) achieves exceptional cycling stability over 1800 h in a Zn//Zn symmetric cell at 5 mA cm −2 . When paired with NVO and I 2 cathodes, the full batteries also deliver remarkable longevity, exceeding 2300 and 11 000 cycles with high specific capacities, respectively.

Article Details

Volume / Issue Vol. 65, Issue 22
Published May 25, 2026
ISSN 1433-7851
Publisher Wiley

Journal Info

Angewandte Chemie International Edition

Wiley

ISSN: 1433-7851 Physical Sciences

Authors (10)

C

Canglong Li

School of Minerals Processing and Bioengineering Central South University Changsha China

T

Tiancheng You

State Key Laboratory of Powder Metallurgy Central South University Changsha China

C

Changding Wang

Institute of Future Technology Southwest Jiaotong University Chengdu China

A

Antai Zhu

State Key Laboratory of Powder Metallurgy

C

Changye Mang

School of Minerals Processing and Bioengineering Central South University Changsha China

H

Huaming Yu

Y

Yang Huang

Guizhou Provincial Key Laboratory of Innovation and Manufacturing for Pharmaceuticals, School of Pharmacy

Y

Yuejiao Chen

G

Guanghui Li

L

Libao Chen

State Key Laboratory of Powder Metallurgy