Choline Iodide‐Mediated Sulfur Conversion and Zinc Plating/Stripping Chemistry in Aqueous Zn–S Batteries

M Mingzhi Qian (National Engineering Research Center of Advanced Energy Storage Materials School of Metallurgy and Environment Central South University Changsha 410083 P.R. China) J Jie Lei (Department of Neurobiology, School of Basic Medicine, Tongji Medical College, Huazhong University of Science and Technology) M Ming Hao Q Qihou Li (National Engineering Research Center of Advanced Energy Storage Materials School of Metallurgy and Environment Central South University Changsha 410083 P.R. China) J Jing Zhan (National Engineering Research Center of Advanced Energy Storage Materials School of Metallurgy and Environment Central South University Changsha 410083 P.R. China) F Fengcheng Tang (National Engineering Research Center of Advanced Energy Storage Materials School of Metallurgy and Environment Central South University Changsha 410083 P.R. China) F Feixiang Wu

Abstract

Abstract Aqueous Zn–S batteries are promising candidates for future energy storage due to their intrinsic safety, environmental friendliness, and low cost. However, their practical application is hindered by sluggish sulfur redox kinetics and rapid zinc anode degradation. Here, we introduce choline iodide (ChI) as a multifunctional electrolyte additive that enables bidirectional catalysis of sulfur conversion and simultaneous protection of the zinc anode. During discharge, Ch + promotes the formation of soluble polysulfide intermediates, which rapidly combine with Zn 2+ to form ZnS via a solid–liquid–solid pathway, accelerating reaction kinetics. During charge, iodine species catalyze the conversion of ZnS back to sulfur. Moreover, Ch + adsorbs on the zinc anode, suppressing dendrite growth and the hydrogen evolution reaction. Importantly, Ch + also inhibits polyiodide shuttling at high iodine concentrations, maximizing catalytic efficiency. Coupled with a CoNC solid‐phase catalyst, the Zn–S cell achieves a record‐low polarization of 0.26 V at 0.1 C, delivers 780 mAh g −1 at 10 C, and maintains 380 mAh g −1 after 5500 cycles.

Article Details

Volume / Issue Vol. 64, Issue 49
Published December 01, 2025
ISSN 1433-7851
Publisher Wiley

Journal Info

Angewandte Chemie International Edition

Wiley

ISSN: 1433-7851 Physical Sciences

Authors (7)

M

Mingzhi Qian

National Engineering Research Center of Advanced Energy Storage Materials School of Metallurgy and Environment Central South University Changsha 410083 P.R. China

J

Jie Lei

Department of Neurobiology, School of Basic Medicine, Tongji Medical College, Huazhong University of Science and Technology

M

Ming Hao

Q

Qihou Li

National Engineering Research Center of Advanced Energy Storage Materials School of Metallurgy and Environment Central South University Changsha 410083 P.R. China

J

Jing Zhan

National Engineering Research Center of Advanced Energy Storage Materials School of Metallurgy and Environment Central South University Changsha 410083 P.R. China

F

Fengcheng Tang

National Engineering Research Center of Advanced Energy Storage Materials School of Metallurgy and Environment Central South University Changsha 410083 P.R. China

F

Feixiang Wu