Li, R., Dawley, R. A., Mishra, S., Adhikari, A., Bol, A. A., Koester, S. J. (2025). WS2 p-MOSFETs with channels deposited by plasma-enhanced atomic-layer deposition. Applied Physics Letters. https://doi.org/10.1063/5.0267728