Shirvani, K., Miraboutalebi, S. V., Kaflou, A., Farvizi, M. (2025). Type-I hot corrosion behavior of Cr-modified slurry aluminide coating superalloy Rene 80. Scientific Reports. https://doi.org/10.1038/s41598-025-25155-5