Jun Gao, Zhenhuan Gao, Xue Fan, Sergei Manzhos, Tongyi Zhang, Yi Liu. "Transfer learning of high-dimensional features via attention-based embedding for Ni-based superalloys." Journal of Applied Physics (2025). https://doi.org/10.1063/5.0271603