Long Hao, Xiaoxin Zhang, Zhiming Fan, Chaoyue Chen, Jianbo Yu, Weidong Xuan, Zhongming Ren. "Significant recrystallization suppression in a nickel-based single crystal superalloy during solution treatment via alternating magnetic field." Applied Physics Letters, 2026. doi:10.1063/5.0305938