Hao, L., Zhang, X., Fan, Z., Chen, C., Yu, J., Xuan, W., Ren, Z. (2026). Significant recrystallization suppression in a nickel-based single crystal superalloy during solution treatment via alternating magnetic field. Applied Physics Letters. https://doi.org/10.1063/5.0305938