Jorit Obenlüneschloß, Nils Boysen, Karl Rönnby, Arbresha Muriqi, Volker Hoffmann, Carlos Abad, Detlef Rogalla, Ulrike Brokmann, Edda Rädlein, Michael Nolan, Anjana Devi. "Rare Mononuclear Lithium–Carbene Complex for Atomic Layer Deposition of Lithium Containing Thin Films." Angewandte Chemie International Edition (2025). https://doi.org/10.1002/anie.202513066