Saravanan Balakrishnan, Selvakumar Subbaiah, Mathew Alphonse, Robert Cep, Sachin Salunkhe, Emad Abouel Nasr. "Investigation of wear behaviour and surface analysis of a coated H13 material for friction drilling application." PLoS ONE, 2025. doi:10.1371/journal.pone.0328168