Meng Zhang, Yanzhu Hu, Binbin Xu, Lisha Luo, Song Wang. "DSF-YOLO for weld defect detection in X-ray images with dynamic staged fusion." Scientific Reports (2025). https://doi.org/10.1038/s41598-025-06811-2